Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 48.1 MPa @Temperature 23.0 °C |
6970 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Porene AN510 Acrylonitrile Butadiene Styrene Applications:injection moldingelectrical appliances such as microwaves, computers, tv, switch boxes, switch panels, etc.automotive componenets |
|||
Tensile Strength, Ultimate | 48.1 MPa @Temperature 23.0 °C |
6970 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Porene KU200 Acrylonitrile Butadiene Styrene Applications:extrusion applicationautomotive parts such as instrument panels, console boxes, switches, automotive louvers, ectelectrical appliances |
|||
Tensile Strength, Ultimate | 48.1 MPa | 6970 psi | ASTM D638 |
SK Chemicals SKYPEL G175D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |