Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4830 MPa
700000 psi
Toho Tenax Besfight® G30-700 12K HTA-7C EP03 Continuous Filament Carbon Fiber
Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car..
Tensile Strength, Ultimate 4830 MPa
700000 psi
Toho Tenax Besfight® G30-700 12K HTA-7C F301 Continuous Filament Carbon Fiber
Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car..