Polymer Property : Tensile Strength, Ultimate = 49.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 49.3 MPa
7150 psi
ASTM D638-95
Multibase Multi-Pro® 3012 RC 30% Glass Filled Polypropylene
Moisture content is 0.06%. Multi-Pro 3012 RC is a glass reinforced polypropylene, chemically coupled which enhances the mechanical properties. This product has been formulated to achieve an esthe..