Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638-95
Multibase Multi-Pro® 0110 X Natural Polypropylene
This product is suitable for moldings incorporating high temperature requirements. This material is specially formulated to be resistant to Copper, but is also resistant to most metals.Data provide..
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638-95
Multibase Multi-Pro® 1010 T Black 10% Talc Content Polypropylene
PPH talc filled compound suitable for containers and wash-tubs requiring elevated stiffness and improved cycle times.Data provided by Multibase.
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638-95
Multibase Multi-Pro® 2005 M 20% Mica Filled Polypropylene
Multi-Pro 2005 M is a mica reinforced polypropylene compound with high stiffness and flex strength. Its high heat resistance lends itself to replace engineered plastics at moderate cost.Data provid..
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638
Quadrant EPP Proteus® LSG HS PP - Heat Stabilized Polypropylene (ASTM Product Data Sheet)
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638
Eastman Tenite Butyrate 285A2R30023 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638
Eastman Tenite Butyrate 485A2R30016 Natural Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness,..
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638
Eastman Tenite Butyrate 530E3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638
Eastman Tenite Butyrate 550E4861316 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638
Eastman Tenite Butyrate 575E3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638
Eastman Tenite Propionate 307A2R30013 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Tensile Strength, Ultimate 33.8 - 40.2 MPa
4900 - 5830 psi
UV Postcure; ASTM D638M
DSM Somos® GP Plus 14122
Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually ..
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638
Devcon Plastic Steel® Liquid (B) Epoxy
General Repair EpoxyComments: Steel-filled liquid epoxy can be cast over models for accurate detail reproduction when making holding fixtures, light-gauge forming dies and molds. Hardens in about a..
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638
Adell EQ-16 Homopolymer Polypropylene, 30% Mica Filled
Data provided by Adell Plastics, Inc.
Tensile Strength, Ultimate 33.8 MPa
4900 psi
BCC Products BC 7062-2H Epoxy Casting
BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi..
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638
Colorite Polymers 3879 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638
Eastman Tenite Butyrate 581A3720016 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Copyright © lookpolymers.com All Rights Reserved