Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 497 MPa

@Temperature 538 °C
72100 psi

@Temperature 1000 °F
Kennametal Stellite Stellite® 3 PM cast
Typical applications include (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) diesel engine exhaust, fluid valve seats, saw cutt..
Tensile Strength, Ultimate 497 MPa

@Temperature 427 °C
72100 psi

@Temperature 801 °F
ASTM E8
ATI Allegheny Ludlum 309 Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..