Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 34.84 MPa | 5053 psi | ASTM D638 |
Ecomass® 1080TU96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b.. |