Tensile Strength, Ultimate 349 MPa
50600 psi
Calculated from tenacity
DuPont™ Nomex® 450 Aramid Staple Fiber
A natural staple fiber. It has higher crystallinity and strength than Type 455 and 462 fibers, and is sold as a 100% meta-aramid staple in various cut lengths. It is used in applications requiring..