Polymer Property : Tensile Strength, Ultimate = 51.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 51.9 MPa
7520 psi
ASTM D638
KKPC Kuhmo GP 150 High Heat Resistant, High Rigidity GPPS
Key features: High Heat-resistance, High Strength Common Uses: Vegetable boxes in refrigerators, humidifiers, lighting apparatus, cassette tape cases, parts of optical instruments, PS paper, etc.GPP..