Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 520 MPa | 75400 psi | Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1 |
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
Tensile Strength, Ultimate | >= 520 MPa | >= 75400 psi | EN 10002-1 |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Ultimate | 520 MPa @Temperature 100 °C |
75400 psi @Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Ultimate | 520 MPa @Temperature 100 °C |
75400 psi @Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms. |
|||
Tensile Strength, Ultimate | 520 MPa @Temperature 816 °C |
75400 psi @Temperature 1500 °F |
|
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 15.9 mm thick bar Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Tensile Strength, Ultimate | 520 - 650 MPa | 75400 - 94300 psi | Minimum Guaranteed |
Industeel CLC 18.10 L General Purpose 18Cr-10Ni Austenitic Stainless Steel Description: CLC 18-10L is a 18Cr-10Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenchi.. |
|||
Tensile Strength, Ultimate | 520 MPa | 75400 psi | |
Industeel CLC 18.10 Nb Niobium Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Nb is a 18Cr-10Ni austenitic stainless steel stabilized with specific Nb addition. This kind of steel is one of the basic grades of the stainless steels range. Niobium bearing and its low c.. |
|||
Tensile Strength, Ultimate | >= 520 MPa | >= 75400 psi | Minimum Guaranteed |
Industeel SIRIUS 800 Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at t.. |
|||
Tensile Strength, Ultimate | 520 MPa | 75400 psi | Annealed prior to test |
Special Metals NILO® Alloy 48 Controlled-Expansion Alloy Inflection point 460°C. A nickel-iron controlled-expansion alloy containing 48% nickel. Its coefficient of thermal expansion is designed to match that of soft lead and soda-lime glasses. The a.. |
|||
Tensile Strength, Ultimate | 520 MPa | 75400 psi | Annealed prior to test |
Special Metals NILO® Alloy K Controlled-Expansion Alloy Inflection point 450°C. A nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, mat.. |
|||
Tensile Strength, Ultimate | 520 MPa | 75400 psi | |
SSAB Tunnplat Domex® 014 BOR Rolled Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Tensile Strength, Ultimate | 520 - 670 MPa | 75400 - 97200 psi | |
SSAB Tunnplat Domex® 460MC HSLA Steel HSLA SteelCharacteristics: Some thicknesses of these steel grades are available with a maximum of 0.03% Si for thin Zn coating. If the material is to be hot-dip galvanized and steel with a maximum .. |
|||
Tensile Strength, Ultimate | 520 MPa | 75400 psi | |
Wieland 1608 Wilaform Gold Universally applicable yellow gold alloy.Applications: casting, chains, laminar decoration, pipes, tubingDental |
|||
Tensile Strength, Ultimate | 520 - 620 MPa | 75400 - 89900 psi | |
CLAL-MSX ARCAP Anticorrosion AP1C H12 1/2 hard, Rolled Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Tensile Strength, Ultimate | 520 - 600 MPa | 75400 - 87000 psi | |
CLAL-MSX ARCAP Anticorrosion AP1 H13 3/4 hard, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Tensile Strength, Ultimate | <= 520 MPa | <= 75400 psi | |
CLAL-MSX ARCAP Anticorrosion AP4 0 Annealed, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Tensile Strength, Ultimate | >= 520 MPa | >= 75400 psi | |
AK Steel ASTM A 607 Class 1 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
Tensile Strength, Ultimate | >= 520 MPa | >= 75400 psi | |
AK Steel SAE J1392, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) AK Steel Formable Grade - F indicates inclusion controlled low alloy.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 520 MPa | 75400 psi | |
Ametek P430L P/M Stainless Steel, Sintered from 7.0 g/cc Green Density Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearite. Sintering was done in dissociated ammonia at 1121°C (2050°F) for .. |
|||
Tensile Strength, Ultimate | 520 - 560 MPa | 75400 - 81200 psi | L direction |
ArcelorMittal Save 20-13 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Ultimate | 520 - 560 MPa | 75400 - 81200 psi | L direction |
ArcelorMittal Save 25-14 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Ultimate | 520 - 560 MPa | 75400 - 81200 psi | L direction |
ArcelorMittal Save 27-15 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Ultimate | 520 - 560 MPa | 75400 - 81200 psi | L direction |
ArcelorMittal Save 30-15 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Ultimate | >= 520 MPa | >= 75400 psi | |
AK Steel ASTM A 1011, Class 2 Formable, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F) Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 520 MPa | 75400 psi | Typical |
ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Annealed Plate, Sheet, and Strip, UNS N04400 Moderately to faintly magnetic at room temperature. Allegheny Ludlum AL 400 alloy is a ductile nickel-copper alloy with resistance to a variety of corrosive conditions. The alloy is most frequentl.. |
|||
Tensile Strength, Ultimate | 520 - 650 MPa | 75400 - 94300 psi | Minimum Guaranteed |
Industeel CLC 18.9 L General Purpose 18Cr-9Ni Austenitic Stainless Steel Description: CLC 18-9L is a 18Cr-9Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenching. This k.. |