Cytec Thornel® T-300 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Tensile Strength, Ultimate 3650 MPa
529000 psi
Cytec Thornel® T-300 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Tensile Strength, Ultimate 3650 MPa
529000 psi
Cytec Thornel® T-300 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor