Polymer Property : Tensile Strength, Ultimate = 54.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 54.9 MPa
7970 psi
ASTM D412
SK Chemicals SKYTHANE® 168D S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Ultimate 54.9 MPa
7970 psi
ASTM D412
SK Chemicals SKYTHANE® S168D Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Copyright © lookpolymers.com All Rights Reserved