Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 569 MPa @Temperature 649 °C |
82500 psi @Temperature 1200 °F |
|
Kennametal Stellite Stellite® STAR with P/M Processing Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfa.. |
|||
Tensile Strength, Ultimate | 569 MPa @Temperature 538 °C |
82500 psi @Temperature 1000 °F |
|
Haynes HR-160® alloy, solution annealed sheet Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Ultimate | 569 MPa @Temperature 316 °C |
82500 psi @Temperature 601 °F |
|
Carpenter Gall-Tough® Stainless Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1.. |