Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 31.0 - 41.0 MPa
4500 - 5950 psi
ASTM D638
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Tensile Strength, Ultimate 35.0 - 41.0 MPa
5080 - 5950 psi
ASTM D638
Kleerdex Kydex® 100 AS Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Anti-static sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for electrical and electronic equipment, medical..