Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 6.41 - 7.25 MPa | 930 - 1050 psi | Tensile shear on aluminum to aluminum; 2.17 MPa on metal to douglas fir; 3.72 MPa on OSB (oriented strandboard) to OSB; 6.76 MPa on plywood to treated lumber |
BASF Master Builders Solutions ChemRex® CX-948 Urethane Adhesive/Sealant Typical applications include high-solids subfloor adhesive, manufacture of windows, doors, and panels, and the assembly of trucks, cabs, and vans.The working open time is 45-60 minutes. The freeze-.. |
|||
Tensile Strength, Ultimate | 6.41 MPa | 930 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 221-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |