Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4.14 MPa
600 psi
Cytec EN-13 (Conap) Casting, Potting, and Molding Compound
High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable..
Tensile Strength, Ultimate 4.14 MPa
600 psi
Cytec EN-14 (Conap) Casting, Potting, and Molding Compound
High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable..
Tensile Strength, Ultimate 4.14 MPa
600 psi
Dow Corning 3-6891 1-PART SILICONE RUBBER ABRADABLE SEALANT COMPOUND
One-part silicone abradable compoundInformation provided by Dow Corning
Tensile Strength, Ultimate 4.14 MPa
600 psi
Bond strength to metal
Dymax Light Weld® 426 High Clarity Glass Bonding Adhesive
Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond..
Tensile Strength, Ultimate 4.14 MPa
600 psi
ASTM D412
AdvanSource Biomaterials ChronoPrene™ 25A Thermoplastic Rubber Elastomer
ChronoPrene™ is a family of biocompatible thermoplastic elastomeric materials.ChronoPrene™ is a family of easy molding, high flow rubber, with excellent chemical resistance to alcohols, acids, and..
Tensile Strength, Ultimate 4.14 MPa
600 psi
BCC Products MB 1150 Polyurethane Foam Modeling Board
MB 1150 is an Avocado colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1150 is low density foam of approximately 15lbs/ft3 board. Easily cut using CNC machining equipment o..
Tensile Strength, Ultimate 4.14 MPa

@Thickness 1.47 mm
600 psi

@Thickness 0.0580 in
Cured; ASTM D638
Aptek 2712-A/B Very low stress silicone adhesive
Very low stress silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space gradeAPTEK 2712-A/B is a two component, white, very soft, thixotropic, electrically insulative, silicone ad..
Tensile Strength, Ultimate 4.14 MPa
600 psi
BCC Products BC 9020 Silicone RTV Rubber
BC 9020 is a violet colored, two-component, flowable compound that regardless of thickness or confinement, cures at room temperature. The cured rubber is high strength and high tear with good elonga..
Tensile Strength, Ultimate 4.14 MPa
600 psi
Loctite® FASTGASKET® 5960 Flange Sealant
Silicone Gasketing and Gasketing and Wire TackersLoctite® Silicone Gasketing materials include unique products with excellent resistance, formulations for high operating temperatures, and UV-curing..