Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 610 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 610 MPa
88500 psi
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4438 High Performance Austenitic Stainless Steel
Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,..
Tensile Strength, Ultimate 610 MPa

@Temperature 400 °C
88500 psi

@Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 4565 High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..
Tensile Strength, Ultimate 610 MPa
88500 psi
Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1
Outokumpu 4828 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Ultimate 610 MPa
88500 psi
Typical
Industeel NUCL 18.10 B4 Natural Boron (Min 1% wt) Alloyed 304 Stainless Steel
Description: Isotope B10 has the property to capture neutrons produced by nuclear reactions. Natural boron contains about 19.9 at% or 18.45 wt % of B10 isotope, the remaining being B11 isotope. NUCL..
Tensile Strength, Ultimate 610 MPa
88500 psi
Haynes 556® alloy, bar after 16000 hours at 648°C
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Ultimate 610 MPa
88500 psi
Annealed prior to test
Special Metals BRIGHTRAY® Alloy 35 Electrical Resistance Alloy
A nickel-iron-chromium electrical-resistance alloy for use at operating temperatures up to 1920°F (1050°C). It is similar to BRIGHTRAY alloy F but with rare-earth additions for greater resist..
Tensile Strength, Ultimate 610 MPa

@Temperature 538 °C
88500 psi

@Temperature 1000 °F
Haynes 230® alloy, GMAW deposit weld metal
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Tensile Strength, Ultimate 610 MPa
88500 psi
0°; ASTM D3039
Polystrand ThermoPro™ IE7010 Unitape Unidirectional Polypropylene-Glass Composite
Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer ..