Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 352 - 421 MPa | 51000 - 61000 psi | |
Eagle Brass 230 Red Brass, 1/2 Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Tensile Strength, Ultimate | 310 - 421 MPa | 45000 - 61000 psi | |
Eagle Brass 260 Cartridge Brass, Annealed Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Tensile Strength, Ultimate | 338 - 421 MPa | 49000 - 61000 psi | |
Eagle Brass 510 Phosphor Bronzes 5% A, 1/4 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |