Tensile Strength, Ultimate 618 MPa
89600 psi
15% Cold Worked
AK Steel 439 ULTRA FORM® Stainless Steel
AK Steel 439 ULTRA FORM™ was developed for applications requiring oxidation and corrosion resistance superior to Type 409 as well as superior formability to AK Steel 439 Stainless Steel. As a resul..