Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 426.1 MPa | 61800 psi | |
IBC Advanced Alloys Beralcast® 310 Beryllium-Aluminum Alloy This alloy, a metal matrix composite, consisting of between 60 and 70% Be (by weight) is a wrought product offered by IBC Engineered Materials to be used in the process of manufacturing extrusions f.. |
|||
Tensile Strength, Ultimate | 426 MPa @Temperature 760 °C |
61800 psi @Temperature 1400 °F |
|
Haynes Hastelloy® N, 1.14 mm sheet, heat treated at 1149°C (2100°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |