Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 370 - 430 MPa | 53700 - 62400 psi | |
ArcelorMittal 260 BH Bake hardening steel, Cold rolled Available in the following: uncoated (HC260B), electroglavanized (HC260B+ZE) and Extragal®/Galvannealed (HC260BD+Z)Description: The composition and processing of these steels are designed to promot.. |