Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 434 - 496 MPa
63000 - 72000 psi
Eagle Brass 230 Red Brass, Hard
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Tensile Strength, Ultimate 434 - 517 MPa
63000 - 75000 psi
Eagle Brass 521 Phosphor Bronzes 8% C, 1/4 Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Tensile Strength, Ultimate 434 - 517 MPa
63000 - 75000 psi
Eagle Brass 735 Nickel Silver 18%, 1/2 Hard
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
Tensile Strength, Ultimate 434 MPa
63000 psi
AK Steel DI-MAX® M-36 Nonoriented Electrical Steel
Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard grades from M-15 to M-47 ..