Tensile Strength, Ultimate 436 MPa

@Temperature 760 °C
63200 psi

@Temperature 1400 °F
Kennametal Stellite Stellite® 31 PM cast
Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous we..