Polymer Property : Tensile Strength, Ultimate = 64.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 64.7 MPa
9390 psi
ASTM D638
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..