Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 640 MPa
92800 psi
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Ultimate 640 MPa
92800 psi
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4439 Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), and cold rolled strip/sheet forms.
Tensile Strength, Ultimate 640 MPa

@Temperature 200 °C
92800 psi

@Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4565 High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..
Tensile Strength, Ultimate 640 MPa

@Temperature 300 °C
92800 psi

@Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4565 High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..
Tensile Strength, Ultimate 640 MPa

@Temperature 200 °C
92800 psi

@Temperature 392 °F
EN min.; EN 10002-5
Outokumpu SAF 2507® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Tensile Strength, Ultimate 640 - 700 MPa
92800 - 102000 psi
Kennametal Stellite Denertiaâ„¢ N19 Nickel Dental Alloy
Denertiaâ„¢ N19 is a low-carbon nickel based porcelain-bonding alloy for the manufacture of dental crowns and bridges.This alloy is Beryllium and Cadmium freeInformation provided by Kennametal St..
Tensile Strength, Ultimate 640 MPa

@Temperature 760 °C
92800 psi

@Temperature 1400 °F
Haynes 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Ultimate 640 MPa
92800 psi
Rm. 200 HB.
Assab Steels 760 Machinery Steel
ASSAB 760 is an easily machinable carbon steel characterized by: Good machinabilityGood mechanical strengthASSAB 760 is primarily intended to be used in the as-delivered condition. It is only to be ..
Tensile Strength, Ultimate 640 MPa
92800 psi
Typical Annealed
ATI Allegheny Ludlum AL 600™ Nickel-Base Alloy, UNS N06600
Allegheny Ludlum is a nickel-chromium alloy designed for use from cryogenic to elevated temperatures in the range of 1093 degrees Celsius. AL 600 alloy is non-magnetic and readily weldable. The al..