Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 647 MPa

@Temperature 538 °C
93800 psi

@Temperature 1000 °F
Haynes Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled
Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit..