Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 675 MPa

@Temperature 204 °C
97900 psi

@Temperature 399 °F
Haynes HR-160® alloy, hot rolled and solution annealed plate
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Tensile Strength, Ultimate 675 MPa
97900 psi
Haynes Multimet® alloy, sand cast, 1171°C heat treatment for 2 hours
Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit..
Tensile Strength, Ultimate 675 MPa
97900 psi
Haynes 25 alloy, vacuum investment castings, solution treated
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Ultimate 675 MPa

@Temperature 540 °C
97900 psi

@Temperature 1000 °F
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Tensile Strength, Ultimate 675 MPa

@Temperature 649 °C
97900 psi

@Temperature 1200 °F
Haynes 230® alloy, hot rolled and 1232°C solution annealed plate
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..