Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 68.3 MPa | 9910 psi | |
Abatron AboCast 8502-7/AboCure 8502-7 Colorless, Low-Exotherm Epoxy Casting Compound AboCast 8502-7/AboCure 8502-7 is a rigid, heat cured, colorless, low-exotherm epoxy casting compound for larger masses. It is a 2-component structural and dielectric liquid system with extremely low.. |