Polymer Property : Tensile Strength, Ultimate = 6820 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 38.0 - 47.0 MPa
5510 - 6820 psi
Average value: 42.5 MPa Grade Count:3
Overview of materials for Nylon 11, Powder
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Powder". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Ultimate 38.0 - 47.0 MPa
5510 - 6820 psi
Arkema Group Rilsan® Fine Powders Grey 49 Polyamide 11
Rilsan® fine powder coatings offer weatherability, long-lasting adhesion, chalk resistance, chemical resistance to aliphatic hydrocarbons, bases, salt solutions, oils, greases and other petroleum p..
Tensile Strength, Ultimate 38.0 - 47.0 MPa
5510 - 6820 psi
Arkema Group Rilsan® Fine Powders Natural Polyamide 11
Rilsan® fine powder coatings offer weatherability, long-lasting adhesion, chalk resistance, chemical resistance to aliphatic hydrocarbons, bases, salt solutions, oils, greases and other petroleum p..
Tensile Strength, Ultimate 38.0 - 47.0 MPa
5510 - 6820 psi
Arkema Group Rilsan® Fine Powders Polyamide 11
Rilsan® fine powder coatings offer weatherability, long-lasting adhesion, chalk resistance, chemical resistance to aliphatic hydrocarbons, bases, salt solutions, oils, greases and other petroleum p..