Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 6836 MPa | 991500 psi | ASTM D1708 |
Daelim H&L Plavis-C CM Conductive Polyimide Bearing Compression Molded. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grad.. |