Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 47.78 MPa
6930 psi
Abatron AboCast 8103-16 One Part Epoxy
One component system. Less viscous than 8103-11. Information provided by Abatron, Inc.Processing: Shelf life 6-8 months at 25°C (77°F). Heat cured; Pot life 360 min. at 100°C (212°C). Peak e..