Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 47.8 MPa
6940 psi
Elastomer Engineering E950-95A Polyurethane
A general-purpose, high-tensile and high-load carrying polyether-based urethane.Information provided by Elastomer Engineering Inc (EEI)