Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 379 - 482 MPa | 55000 - 69900 psi | |
Ametek AM 388™ Alloy (UNS C72650) TB00 Solution HT Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |