Polymer Property : Tensile Strength, Ultimate = 7.853 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 7.853 MPa
1139 psi
Dow Corning SILASTIC® 24043-V SILICONE RUBBER BLUE
80 Durometer, peroxide cured, high strength Silicone Rubber Compound.Information provided by Dow Corning