Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 487 MPa @Temperature 538 °C |
70600 psi @Temperature 1000 °F |
|
Haynes Multimet® alloy, sand cast, 1171°C heat treatment for 2 hours Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Tensile Strength, Ultimate | 487 MPa @Temperature 260 °C |
70600 psi @Temperature 500 °F |
Plate |
AK Steel NITRONIC® 30 Austenitic Stainless Steel AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi.. |