Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 441.2 - 490 MPa | 63990 - 71100 psi | |
International Mold Steel Porcerax II Sintered, Porous Mold Steel Description: Porcerax II is a sintered, porous metal with porosity in the range of 20 to 30% by volume. A system of interconnected pores with an average diameter of 7 or 20 micron is dispersed throu.. |
|||
Tensile Strength, Ultimate | 420 - 490 MPa | 60900 - 71100 psi | |
SSAB Tunnplat Aluzink 350A YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is .. |
|||
Tensile Strength, Ultimate | 420 - 490 MPa | 60900 - 71100 psi | |
SSAB Tunnplat Dogal 350YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur.. |
|||
Tensile Strength, Ultimate | 420 - 490 MPa | 60900 - 71100 psi | |
ArcelorMittal HSLA 340 High strength low alloy steel for cold forming, Cold Rolled Available in the following: uncoated (HC340LA), electroglavanized (HC340LA +ZE) and Extragal®/galfan/Galvannealed (HC340LA+Z/+ZA/+ZF)Description: Steels in the HSLA (High Strength Low Alloy) range .. |