Polymer Property : Tensile Strength, Ultimate = 721.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 721.9 MPa
104700 psi
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Plate 0.500 in (12.7 mm)
Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.500 inch plate. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu..