Polymer Property : Tensile Strength, Ultimate = 75.08 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 75.08 MPa
10890 psi
BCC Products MB 4000 RED Urethane Foundry Plank
MB4000 Red is an extremely tough, high impact Urethane Plank, that can replace aluminum and other metals for many foundry applications. Features: excellent machinability, low dust emission, mostly ..