Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 5.17 MPa
750 psi
TM R050-36
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin
Resinlab™ EP1295 Black is a medium viscosity, halogen free, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (..
Tensile Strength, Ultimate 5.17 - 97.0 MPa
750 - 14100 psi
Average value: 33.7 MPa Grade Count:31
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Ultimate >= 5.17 MPa
>= 750 psi
ASTM D412
Multibase Multi-Flex® TPE A 6221 LA BLK
Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Tensile Strength, Ultimate 5.17 MPa
750 psi
Dry weak gel; ASTM D412
Lubrizol Estane® ALR G2000 Water Absorbent Thermoplastic Polyurethane
Type: Estane® ALR G2000 is an aliphatic thermoplastic polyurethane (TPU) resin designed to absorb water and transport moisture.Features: Contains UV additivesAvailable in AmericasInformation Provid..
Tensile Strength, Ultimate 5.17 MPa
750 psi
Side 2 Silicone Property; ASTM D412
Arlon 19646B025 Silicone Rubber/Fiberglass Laminate
Side 1:cured silicone rubber; Substrate: 1523 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil Polyethylene
Tensile Strength, Ultimate 5.17 MPa
750 psi
BCC Products BC 9040 T Silicone RTV Rubber
BC 9040T is a clear, addition/platinum cure, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high..
Tensile Strength, Ultimate 5.17 MPa
750 psi
ASTM D638
Multibase Multi-Flex® A 6221 C TPE Thermoplastic Elastomer
Forms: PelletsInformation provided by Multibase