Polymer Property : Tensile Strength, Ultimate = 75900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 523 MPa
75900 psi
Kennametal Stellite Stellite® STAR with P/M Processing
Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfa..
Tensile Strength, Ultimate 523 MPa

@Temperature 649 °C
75900 psi

@Temperature 1200 °F
Haynes HR-160® alloy, hot rolled and solution annealed plate
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..