Polymer Property : Tensile Strength, Ultimate = 7693 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 53.04 MPa
7693 psi
Peak; Ambient Cure
Reltek BONDiTâ„¢ B-536 Adhesive System
Key Properties: Very high strength bonding of dissimilar materials.High moisture and solvent resistance.Fast ambient cure with good pot life.Ease of use.Applications: Outstanding adhesive for very h..