Polymer Property : Tensile Strength, Ultimate = 7730 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 53.3 MPa
7730 psi
ASTM D638
Plenco Valite 4224 Novolac Phenolic, Granular, Transfer Molded  (discontinued **)
This Valite product has been replaced by Plenco 4224. Data provided by Plenco.VALITE 4224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability ch..