Polymer Property : Tensile Strength, Ultimate = 78300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 500 - 540 MPa
72500 - 78300 psi
after heat treatment
PEAK Werkstoff DISPAL S691 Aluminum Alloy, AlCu5Ti
High stiffness and elongation at ruptureInformation provided by PEAK Werkstoff GmbH
Tensile Strength, Ultimate 410 - 540 MPa
59500 - 78300 psi
Materion Beryllium Copper Alloy 25 Strip; A -Planished (TB00) Temper (UNS C17200)
Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 46-67Tabulated properties apply ..
Tensile Strength, Ultimate 400 - 540 MPa
58000 - 78300 psi
Materion Beryllium Copper Alloy 25 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17200)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 400 - 540 MPa
58000 - 78300 psi
Materion Beryllium Copper Alloy M25 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17300)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 480 - 540 MPa
69600 - 78300 psi
SSAB Tunnplat Aluzink 380A YP High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is ..
Tensile Strength, Ultimate 360 - 540 MPa
52200 - 78300 psi
Rm
ALIMEX PLANAL 7075 T651/T652 Aluminum Alloy
Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machi..