Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 79.4 MPa | 11500 psi | ASTM D1708 |
Daelim H&L Plavis-N DF Unfilled Aromatic Polyimide Bearing Direct Formed. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS polyimi.. |