Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 796 MPa | 115000 psi | |
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 704°C (1300°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man.. |
|||
Tensile Strength, Ultimate | 796 MPa | 115000 psi | |
Haynes Hastelloy® N, 1.6 mm sheet, aged 128 hours at 815°C (1500°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |