Polymer Property : Tensile Strength, Ultimate = 8.693 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 8.693 MPa
1261 psi
MIL-H-83282 fluid immersion, 70 hrs. at 275°F; ASTM D1414
Freudenberg Simrit N456 Nitrile Elastomer (NBR)
General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings