Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 803.2 MPa
116500 psi
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Sheet 0.125 in (3.2 mm)
Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.125 inch sheet. Other property values are typical of INCONEL® alloy 686.Data provided by the manufacture..