Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 807 MPa | 117000 psi | RT, Dry, 90° Direction |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ S2-Glass Fabric MVK-14 Polyimide Astroquartz and S2 glass prepregs are an affordable, easy-to-process material for high-temperature radome and antenna applications. MVK-14 is a non-MDA alternative to BMI, cyanate e.. |
|||
Tensile Strength, Ultimate | 807 MPa | 117000 psi | |
Universal Wire Works 617 Nickel Alloy Welding Wire Alloy 617 is used for TIG and MIG welding of Inconel type alloy 617 and alloys of similar composition. Alloy 617 welds produce high stress-rupture strength in prolonged exposure to high temperatures.. |