Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 83.4 MPa
12100 psi
ISO 527
Polikim KESTAMID® PA6G Polyamide 6
Kestamid® is also known as Cast Polyamide or Cast Nylon. Kestamid® is an engineering plastic used commonly in all industrial branches for its superior mechanical, physical, chemical and electrical..
Tensile Strength, Ultimate 83.4 MPa
12100 psi
DIN 53455; ASTM D638
Kolon SPESIN® KP213G15HI Multi Reinforced PBT Resin  (discontinued **)
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea..
Tensile Strength, Ultimate 83.4 MPa
12100 psi
DIN 53455; ASTM D638
Kolon KOPA® KN1322VO Flame Retardant Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Tensile Strength, Ultimate 83.4 MPa
12100 psi
DIN 53455; ASTM D638
Kolon KOPA® KN3311 General Purpose Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Tensile Strength, Ultimate 83.4 MPa
12100 psi
DIN 53455; ASTM D638
Kolon KOPA® KN3311N General Purpose Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Tensile Strength, Ultimate 83.4 MPa
12100 psi
ASTM D638
SK Chemicals SKYTHANE® U1731C Magnetic Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 83.4 MPa

@Temperature 871 °C
12100 psi

@Temperature 1600 °F
Longitudinal
AK Steel NITRONIC® 19-D Duplex Stainless Steel
AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}), good drawing and welding characteristi..