Tensile Strength, Ultimate 57.4 MPa
8330 psi
ASTM D638
Plenco 4100 Phenolic, Granular, Injection Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in appliance and ..
Tensile Strength, Ultimate 57.4 MPa
8330 psi
ASTM D638
Plenco Valite 424 Novolac Phenolic, Granular, Injection Molded  (discontinued **)
This Valite product has been replaced by Plenco 2424. Data provided by Plenco.VALITE 424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a ..