Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 602 MPa

@Temperature 538 °C
87300 psi

@Temperature 1000 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..